性能项目试验条件[状态]测试方法测试数据数据单位 |
基本性能吸水率23℃,24小时ASTM D-570% |
物理性能泰伯磨耗量1000g,CS-17ASTM D-1044mg/1000次 |
比重ASTM D-792 |
机械性能IZOD冲击强度无缺口1/2",23℃kg.cm/cm |
IZOD冲击强度-40℃,无缺口1/2kg.cm/cm |
断裂伸长率23℃ASTM D-638% |
搞剪强度23℃ASTM D-732Kg/cm2 |
挠曲强度80℃ASTM D-790Kg/cm2 |
挠曲强度-40℃ASTM D-790Kg/cm2 |
洛氏硬度23℃ASTM D-785 |
抗拉屈服强度23℃ASTM D-638Kg/cm2 |
抗拉屈服强度80℃ASTM D-638Kg/cm2 |
抗拉屈服强度-40ASTM D-638Kg/cm2 |
挠曲模量-40℃ASTM D-790Kg/cm2 |
抗拉断裂强度23℃ASTM D-638Kg/cm2 |
挠曲模量23℃ASTM D-790Kg/cm2 |
压缩强度23℃ASTM D-695Kg/cm2 |
洛氏硬度23℃ASTM D-785 |
挠曲强度23℃ASTM D-790Kg/cm2 |
挠曲模量80℃ASTM D-790Kg/cm2 |
IZOD冲击强度23℃,无缺口1/8kg.cm/cm |
电气性能体积电阻率ASTM D-257无水|3.5%水 | 1014-1015|1011-1012 | Ω.cm |
损耗因素106HzASTM D-150 |
介电强度1/8"ASTM D-149KV/mm |
损耗因素50HzASTM D-150无水|3.5%水 | 无水|3.5%水 | 0.07|- | 50Hz|- | |
IEC导电径踪指数UL 746V |
介电常数106HzASTM D-150 |
损耗因素103HzASTM D-150 |
抗电弧性1/8"ASTM D-150 |
介电常数50HZASTM D-150 |
介电常数106HzASTM D-150 |
热性能导热系数Kcal/m.hr.°C |
线性热膨胀系数ASTM D-69610-5cm/cm.℃ |
比热Cal/g.°C |
热挠曲温度ASTM D-648℃ |
熔点差示扫描测热计DSC法℃ |
UL-94抗燃级UL 94 |
热挠曲温度18.6kg/cm2ASTM D-648℃ |